Properties Grade | Max Energy Product | Remanence | Coercive Force | Intrinsic Coercive Force | Density | Relative Recoil Permeability | Temp Coeff | Max. Working Temp |
(BH)max | Br | Hcb | Hcj | D | α Br | Tw | ||
KJ/m3(MGOe) | T | KA/m(KOe) | KA/m(KOe) | g/cm3 | μ r | %/ ℃ | ℃ | |
BNI-3 | 8-24(1.0-3.0) | 0.20-0.40 | 120-240(1.5-3.0) | 480-640(6.0-8.0) | 3.9-4.4 | 1.2 | -0.15 | 100 |
BNI-4 | 28-36(3.5-4.5) | 0.40-0.46 | 250-335(3.1-4.2) | 575-735(7.2-9.2) | 4.2-4.9 | 1.2 | -0.13 | 110 |
BNI-5 | 37-44(4.6-5.5) | 0.45-0.51 | 280-360(3.5-4.5) | 640-800(8-10) | 4.5-5.0 | 1.2 | -0.13 | 120 |
BNI-6 | 44-52(5.5-6.5) | 0.51-0.56 | 295-375(3.7-4.7) | 640-800(8-10) | 4.7-5.1 | 1.13 | -0.11 | 120 |
BNI-6H | 40-52(5.0-6.5) | 0.48-0.56 | 335-400(4.2-5.0) | 1035-1355(13-17) | 4.8-5.2 | 1.13 | -0.15 | 130 |
BNI-7 | 51-59(6.5-7.5) | 0.54-0.64 | 320-400(4.0-5.0) | 640-800(8-10) | 5.0-5.5 | 1.13 | -0.11 | 120 |
BNI-5SR(PPS) | 36-44(4.5-5.5) | 0.45-0.50 | 300-360(3.8-4.5) | 875-1115(11-14) | 4.9-5.4 | 1.13 | -0.13 | 150 |